Test result

The results table in the temperature cycling report records 84% capacity retention after 4,000 cycles at 25 °C for the tested 32700/6000 LiFePO₄ cell, batch H05. The test used 1C charge and 1C discharge. Retention is relative to the initial capacity measured at the same temperature.

Test method and evidence location

The workbook lists the test date as 20 August 2024. Its non-standard sample test uses 1C constant-current/constant-voltage charging to 3.65 V with a 0.03C cutoff, 10-minute rests, and 1C constant-current discharge to 2.0 V. The result applies to the tested sample and the reported protocol.

Open the worksheet 报告 (Report), then find the capacity-retention table in the results section 测试结果. Read the intersection of the 4,000-cycle row and the 25 °C column.

Download the original cycling test report (XLS)

Résultat de l’essai

Le tableau de la feuille « 报告 » indique que la cellule LiFePO₄ 32700/6000 du lot H05 a conservé 84 % de sa capacité initiale à 25 °C après 4 000 cycles, avec une charge et une décharge à 1C. Le résultat concerne l’échantillon et le protocole d’essai décrits dans le rapport.